Grade | C | Mn | Si | S | Cu | Fe | Ni |
---|---|---|---|---|---|---|---|
Monel 400 | 0.30 max | 2.00 max | 0.50 max | 0.024 max | 28.00 – 34.00 | 2.50 max | 63.00 min |
Grade | C | Mn | Si | S | Cu | Fe | Ni |
---|---|---|---|---|---|---|---|
Monel K500 | 0.25 max | 1.5 max | 0.5 max | 0.010 max | 27.00 – 33.00 | 0.5 – 2 | 63.00 min |
Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
---|---|---|---|---|---|
Monel 400 | 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80,000 , MPa – 550 | Psi – 35,000 , MPa – 240 | 40 % |
Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
---|---|---|---|---|---|
Monel K500 | 8.44 g/cm3 | 1350 °C (2460 °F) | Psi – 160000 , MPa – 1100 | Psi – 115000 , MPa – 790 | 20 % |