Grade | C | Fe | S | Cu | Ni | Mn | Si | Cr |
---|---|---|---|---|---|---|---|---|
400 | 0.15 | 6.00 – 10.0 | 0.015 | 0.50 | 72.00 | 1.00 | 0.50 | 14.00 – 17.00 |
Grade | Si | S | C | Mn | Cu | Fe | Ni |
---|---|---|---|---|---|---|---|
Monel K500 | 0.5 max | 0.010 max | 0.25 max | 1.5 max | 27.00 – 33.00 | 0.5 – 2 | 63.00 min |
Element | Melting Point | Density | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
---|---|---|---|---|---|
Monel 400 | 1350 °C (2460 °F) | 8.8 g/cm3 | Psi – 35,000 , MPa – 240 | Psi – 80,000 , MPa – 550 | 40 % |
Density | Yield Strength (0.2%Offset) | Melting Point | Elongation | Tensile Strength |
---|---|---|---|---|
8.44 g/cm3 | Psi – 115000 , MPa – 790 | 1350 °C (2460 °F) | 20 % | Psi – 160000 , MPa – 1100 |