Grade | C | P | S | Cr | Mn | Si | Mo | Ni | Fe | N |
---|---|---|---|---|---|---|---|---|---|---|
Duplex S31803 | 0.030 max | 0.030 max | 0.020 max | 22 – 23 | 2 max | 1 max | 3 – 3.50 | 4.50 – 6.50 | Bal | 0.14 – 0.20 |
Grade | C | Mn | Si | Cr | Mo | Ni | P | S | N | Fe |
---|---|---|---|---|---|---|---|---|---|---|
2507 | 0.030 max | 1.20 max | 0.80 max | 24.00 – 26.00 | 3.00 – 5.00 | 6.00 – 8.00 | 0.035 max | 0.020 max | 0.24 – 0.32 | 58.095 min |
Density | Tensile Strength | Melting Point | Yield Strength (0.2%Offset) | Elongation |
---|---|---|---|---|
7.8 g/cm3 | Psi – 116000 , MPa – 800 | 1350 °C (2460 °F) | Psi – 80000 , MPa – 550 | 15 % |
Grades | Density (lb/in 3) | Density (g/cm 3) | Melting Point (°C) | Melting Point (°F) |
---|---|---|---|---|
2507 | 0.281 | 7.8 | 1350 | 2460 |